Tom Bubenik, Steven Polasik, Benjamin Hanna
DNV, Dublin, USA
Abstract
Effective area calculations are used to identify which corrosion depth measurements control the failure pressure of a cluster of metal-loss anomalies reported by an in-line inspection (ILI). The depth measurements usually correspond to individual anomalies that are grouped together based on defect interaction criteria. The effective area calculations determine an effective length and depth based on the ILI reported cluster and box lengths and depths at the time of the inspection. As corrosion growth occurs, though, the depths of some or all of the individual anomalies within a cluster can increase. As a result, the effective length of the cluster can increase or decrease.
Growth of individual anomalies within a cluster is often non-uniform, with some anomalies increasing in depth (and possibly length) more quickly than others. As a result, local “hot spots” can develop and eventually dominate the effective area calculations. Understanding how corrosion growth affects the effective dimensions of a cluster is important in estimating remaining lives and determining which clusters are most likely to fail first. The flaw geometry at failure depends on the local operating pressure, the corrosion growth rates, and the initial cluster geometry.
Remaining life calculations depend on reliable estimates of both initial and final metal loss depths and lengths. Because differences between individual metal loss box corrosion growth rates can affect effective flaw dimensions, accuracy is important. Initial corrosion depths and lengths are reasonably well known from typical ILIs. Overestimating or underestimating the flaw geometry at failure under operating conditions can lead to overly conservative or unconservative remaining life predictions.
This paper evaluates the effects of corrosion growth on the effective dimensions, flaw geometries at failure, and remaining lives of clusters. The authors examine 20 real-world clusters ranging in length from short to long and containing few to many individual anomalies. The authors determine when and how each cluster’s effective length and critical depth changes as corrosion growth takes place along the cluster until it reaches a failure condition at the local operating pressure. Then, they evaluate how the changes in effective lengths and critical depths affect remaining life predictions. Conclusions regarding how to best estimate remaining lives of clustered anomalies are developed and documented.
KEYWORDS: Engineering analysis, ILI analysis, ILI applications, Corrosion studies