Recent work considered the factors controlling SCC and typical cracking speeds based on laboratory test data to identify the factors and quantify the laboratory speeds, which it used to formulate bathtub speed curves that compared favorably to typical field cracking speeds. This paper adds significantly to the hundreds of cracks in the field dataset considered previously. Traits typical of the field cracking are trended and compared with current ILI crack-tool reporting criteria to identify their strengths and potential weaknesses concerning safety and reliability.
Fracture features typical of ruptures and major spills due to SCC are contrasted to those evident for leaks and larger secondary cracking, for benign field cracking, and finally for field cracking at the scale of the steel’s microstructure. It is shown that regardless of the scale the recurrent traits of failures causing ruptures and major spills are comparable down to the smallest of cracking – indicating that the mechanics of SCC is scalable. The associated crack populations are then trended relative to their spacing and sizing as evident on the pipe’s OD surface, on its fracture surfaces, or in x-sections of intact cracking. The resulting populations of surface lengths and profiled depths are then trended for well in excess of a 1000 cracks. That population was then parsed based on their sizes and field response as 1) benign, 2) secondary cracks remote to ruptures and major spills, 3) larger secondary cracks adjacent to ruptures and major spills, leaks and smaller spills, and finally 4) ruptures and major spills.
The parsed dataset was then trended relative to a normalized form of crack aspect ratio as a function of normalized of depth, which effectively discriminated between each of the four parsed datasets. The usual crack-tool reporting criteria specified relative to length and depth were then recast as a function of pipe diameter and wall thickness, such that they could be contrasted with the field data. This identified what amongst this field population would be reported if the tool successfully identified and called each of the cracks. The results showed that the current criteria cull the benign cracking and the smaller secondary features, and report all outcomes that led to ruptures and major spills. Thus, the reporting criteria avoid digs for benign cracking, and successfully capture cracking that poses immediate concern for failure. While effective as just noted, portions of the population that are reaching sizes that have posed a threat in past are less effectively reported. The results indicate that depth is not a key factor in this outcome – rather it was controlled by crack length. This, coupled with the observation that crack length is underreported to an extent controlled by aspect ratio, suggests improved safety and reliability could be affected significantly by improvements in length sizing and length reporting. These aspects are elaborated further in the paper.
KEYWORDS FOR SUBJECT AREA: Crack assessment, ILI applications
Available after the event