Abstract

SONACOL owns and operates a 135 km, 6-inch diameter pipeline refined products pipeline located in Chile, which was constructed in 1964 from longitudinally welded (ERW) pipe with thicknesses between 5.16 and 12.7 mm. This pipeline has been inspected on multiple occasions for metal loss, deformations and cracks as part of its Integrity Management Plan. Following the most recent inspection and subsequent integrity assessment, an operational pressure reduction was introduced as some of the reported dents were considered to pose an immediate threat to the pipeline integrity. Of particular concern were dents identified to be associated with brittle longitudinal seam welds.

SONACOL supported by ROSEN have developed a strategy to assure the continuous safe operation of this pipeline. This involved a full scale testing and various levels of assessment increasing in complexity.

The strategy included the selection of critical dents, which were removed from the pipeline and underwent a full-scale fatigue testing, NDT assessment and material characterisation tests. Testing results demonstrated an acceptable level of conservatism in the assessment methods since fatigue growth was found to be overestimated. Dents were prioritised using an initial EPRG fatigue assessment followed by an FEA assessment. Additionally, the API 1183 longitudinal weld interaction was used to determine the likely effect of welds on the fatigue life of dents. The integrity assessment, which incorporated all ILI reported features including crack like anomalies, was used to develop a refined repair plan. This strategy has allowed Sonacol to continue operating the pipeline and demonstrate a suitable safety margin for that.

This paper summarises the different stages through the process of developing the dent management strategy.

Read/Download PaperGradeAvailable after the event