1Baker Hughes, Cramlington, UK. 2Baker Hughes, Houston, USA. 3Baker Hughes, Calgary, Canada
Selective Seam weld Corrosion (SSWC) is a long-standing, known threat to pipeline integrity. With the comprehensive amendments to the Pipeline Safety Regulations (Code of Federal Regulations CFR, part 192) issued by the U. S. Pipeline and Hazardous Materials Safety Administration (PHMSA), there has been an increased focus on understanding this threat and other seam weld defects within operator pipelines.
According to the Pipeline Research Council International (PRCI), SSWC is defined as: "Accelerated corrosion of or near the bond line in autogenous welds, resulting in a groove-like feature that often coincides with shallower corrosion extending beyond the limits of the longitudinal seam."
Due to its distinctive morphology, SSWC poses a significant threat to the integrity of high-pressure pipelines, as its length-to-depth ratio significantly reduces its failure pressure over time. The interaction of SSWC with other pipeline defects, such as surrounding corrosion, dents, bends and strain, can increase integrity risk.
Given the very axially oriented narrowness and steep sided nature of SSWC, a Transverse Field inspection technology is best suited to detect SSWC, where the magnetic flux intersects the steep side of the defect perpendicularly. Transverse Inspection Vehicles, by design, are targeting the axially narrow defects and are not necessarily optimal for the “Shallower corrosion extending beyond the limits of the longitudinal seam”.
The author has been inspecting pipelines using Transverse inspections since 1997. During this period, high-field Transverse inspection has detected cracks (with openings greater than 0.2 mm), SSWC, and preferential seam weld corrosion. Combining the results from Tri-axial Axial Magnetic inspection, high-resolution caliper, Inertial Mapping and Strain data, has allowed for comprehensive reporting of seam weld and spiral weld defects.
This paper presents a comprehensive evaluation of SSWC and other seam weld defects through the lens of Inline Inspection (ILI) technologies, including examples that leverage the multiple ILI data streams and technologies, and will share results from operational digs and quantitative industrial testing via pull-through testing.
Available after the event