1Elsyca, WIjgmaal, Belgium. 2Enbridge, Stockbridge, USA
Pipeline’s integrity is typically assessed by overline cathodic protection (CP) surveys and in-line inspection (ILI) runs. The overline surveys are based on ON/OFF potential readings at discrete test station locations. The criterion of -850mV OFF potential according to NACE SP 0169 standard and 15V AC voltage according to NACE SP 177 is only indicative for the corrosion risk of the pipeline and measurements are limited in space and time. They do not provide corrosion rates for determining the severity of the corrosion attack. ILI runs require feature recognition and mapping for corrosion growth rate calculations and do not reveal the root cause of the observed features.
Physic based computer modeling bridges the CP surveys with ILI runs by converting the potential readings to corrosion rates. Corrosion rate is calculated from the computed current density at coating defects that are sized based on the corrosion feature size (width x length). The computer models are calibrated by comparing the simulated pipe-to-soil potentials and AC voltage with the voltage reads. Metal loss and corrosion growth rate is calculated after rerunning the model with the latest annual surveys. As such the impact of events that jeopardize pipeline’s integrity is quantified allowing operators to correct their corrosion prevention strategy.
A case study will be discussed on a 85 mi long 12” pipeline with fusion bonded epoxy (year 2014) and coal tar enamel (year 1965) coating under DC and AC interference from third party systems. Computer models were utilized to compute metal loss and the risk for stress corrosion cracking based on historical CP data. Results were compared with latest ILI run.
Available after the event