1First Gas Limited, New Plymouth, New Zealand., 2Quest Integrity NZL Limited, Wellington, New Zealand
Abstract
First Gas operates the natural gas transmission pipeline network in New Zealand. In 2022, crack-like linear indications on the long seam of the pipeline were identified by non-destructive testing (NDT) carried out opportunistically during coating refurbishment of a length of pre-1971 pipeline. Quest Integrity were engaged to investigate these crack-like linear indications. Metallurgical analysis of coupons removed from the pipeline concluded that the crack-like linear indications observed were Selective Seam Weld Corrosion (SSWC). With knowledge of this new threat, First Gas initiated a work program to manage this risk in the pipeline.
The work program included a Like-and-Similar analysis of the three most recent Magnetic Flux Leakage (MFL) metal loss ILI data sets collected in the pipeline and metallurgical analysis results, and additional field verification using advanced ultrasonic methods to further characterize metal loss features interacting with the long seam. Corrosion growth rates determined from the Like-and-Similar analysis and characterization of features detected ultrasonically and/or metallurgically verified were utilized in a Fitness-for-Service and remaining life assessment of external metal loss features, both interacting with and away from the longitudinal seam weld.
First Gas used the results obtained from the above investigation to update their integrity management plan for their pre-1971 pipelines, now including management of the threat posed by SSWC. This paper presents the full scope of work performed by First Gas and Quest Integrity to manage the threat posed by SSWC for the pre-1971 pipelines and shares the learnings obtained from the process.
Keywords: ERW pipe, Pipeline integrity management, Corrosion, Selective Seam Weld Corrosion, Crack-Like Features