Instrumented Indentation Testing (IIT) is a non-destructive technique used to estimate mechanical properties such as yield strength and ultimate tensile strength of materials, making it a useful tool in the assessment of pipeline steels. Although the importance of surface preparation for accurate IIT measurements is widely recognized, published systematic studies evaluating the specific effects of varying surface finishes on IIT results are rare. Identifying the potential implications of over- or under-preparation could help ensure more efficient and accurate IIT.
In this study, the impact of different surface finishes, ranging from 280 grit to 2000 grit, on the yield strength measurements of pipeline steel using IIT was investigated. Various locations on the pipe were ground and polished to these target surface finishes, and IIT was performed at each location. Metallographic cross-sections were prepared from the locations of different surface finishes with IIT indents to analyze the influence of surface preparation.
Preliminary results indicate that IIT measurements taken at a 1200 grit surface finish are more consistent with the yield strength values obtained from destructive transverse tensile tests. In contrast, IIT results at 280 grit exhibited yield strength values significantly higher than those from tensile testing, while measurements at 2000 grit showed lower yield strength values in some cases, which could be attributed to polishing parameters such as the pressure applied during the polishing process and the polishing time. Metallographic analysis suggests that the rough surface at 280 grit and the formation of surface voids at 2000 grit may have contributed to these discrepancies.
This ongoing experimental work aims to establish a conclusive understanding of the relationship between surface finish and IIT measurements, potentially identifying an optimal surface preparation technique that ensures reliable IIT data without unnecessary refinement efforts.
KEYWORDS: IIT, Surface Preparation, Polishing, Yield Strength, Material Properties Verification