Abstract
This research and development are for the purpose of optimizing an In-line inspection (ILI) system for the detection, characterization, and sizing of selective seam weld corrosion (SSWC). This technology utilises both Axial Flux Leakage (AMFL) and Circumferential Magnetic Flux Leakage (CMFL) measuring systems. The technology is also designed to take up to 1,600 readings per square inch providing the required resolution to detect and size SSWC.
This paper will present several phases of the study that include conceptual development, pull testing, and field verification from live runs on pipeline systems containing SSWC. It includes the development of software and analysis tools that utilize varying signal responses to both AMFL and CMFL for different metal loss geometries.
The evaluation of SSWC, and of general corrosion coinciding with the long seam weld area, requires both AMFL and CMFL ILI data that has been collected with very high resolution. This research shows that field-tool correlation improves when the process of characterization and sizing SSWC is carried out in the following three steps:
1. The use very high-resolution data to better delineate SSWC from within the general corrosion area, and to provide precise positioning of the long seam weld.
2. Determine whether the long seam corroded areas exhibit wedge, groove, or axial slot like shapes that are typical of SSWC. These features are frequently in aeras of significant corrosion adding to the complexity of characterization and sizing.
3. Apply both AMFL and CMFL sizing algorithms to the preselected SSWC locations to properly size axially orientated wedge or groove-like features.
This paper will also illustrate additional challenges found during field verifications. These include the occurrences metal loss coinciding with seam flaws such as lack of fusion and hook crack flaws, and the current development of analysis tools that address these compounded flaws that can, on occasion be misclassified as SSWC.
Available after the event