Pipelines that operate at elevated temperatures present unique challenges to composite repair applications. The material performance of a composite repair is impacted both by its cure temperature and the operating temperature. These variations collectively influence the pressure capacity of the applied composite system.
The first question explored in this paper is the degree to which the properties of a composite system, specifically the tensile strength and modulus, change at various elevated temperatures compared to ambient temperatures. The second question explored in this paper is how the cure temperature of the composite affects the tensile strength and modulus at various temperatures. An elevated temperature post-cure will increase the crosslink density of the polymer, which should result in a stronger, stiffer cured material. Increased crosslink density will also likely affect the elevated temperature properties of the composite repair system.
The testing program referenced in this paper developed a protocol to evaluate the abovementioned questions. Two commercially available, carbon fiber-based composite repair systems were tested. Each system was tested for tensile strength and modulus at various temperatures, from 70oF – 250oF. All samples were analyzed based on tensile strength, yield strength, glass transition temperature (Tg), and ductility on a stress/strain curve. The full test protocol was performed on both composite repair systems at three different cure temperatures. Ultimately, the intent of this testing program was to evaluate how the properties of composite repair systems change at elevated temperatures and to explore how variations in a composite’s cure temperature affect these properties.
Available after the event