292

Kenneth George1, Sergio Limon1, Daniel Gutierrez2, Ryan Milligan1, USA.2

1Blade Energy Partners, Houston, USA. 2Phillips 66, Houston, USA

An increasing number of pipeline segments are in-line inspected every year for the presence of cracking and seam weld anomalies. While not all planar indications reported by in-line inspection systems pose a safety concern to the integrity of a pipeline, an engineering assessment can assist in identifying and prioritizing which indications to investigate and remediate. One key input in the engineering assessment is the determination of the pipeline’s fracture toughness, a material property that can be measured and quantifies the resistance of the pipeline to crack extension and fracture. To accurately measure this parameter, specialized sub-scale specimen geometries and standardized testing procedures have been published in the industry.

In this study, the fracture toughness of steel line pipe using miniature compact tension (CT) specimens with a ratio width-to-thickness, W/B = 2, unflattened, and side grooved was measured. These test specimen conditions led to a limited test ligament area, magnifying the influence of inherent weld material inclusions, crack tip constraint, and test set up fidelity on the measured toughness. Testing focused on characterizing the lower-bound J-R resistance curve of the seam weld using both displacement-controlled and crack opening displacement (COD)-controlled methods. While displacement control is commonly used, it poses a significant challenge for miniature test specimens due to the sudden release of elastic energy at peak load, which can trigger uncontrolled tearing and compromise data validity. In contrast, COD control offers a more stable crack propagation regime by dynamically compensating for stored energy changes at the onset of unstable crack advance. However, it requires precise tuning and robust error detection.

The material under investigation was an electric resistance welded (ERW) API 5L X60, with a 12-inch nominal outside diameter and a 0.312-inch wall thickness. Results suggest that while ASTM E1820-compliant subsize CT testing is feasible, it requires careful control and interpretation. Post-test SEM examination was conducted to distinguish between fracture mechanisms such as cleavage, material inclusion-driven fracture, crack tip over-constraint, and stable ductile tearing.

Read/Download PaperGradeAvailable after the event