1DarkVision, North Vancouver, Canada, 2Flint Hills Resources, Wichita, USA
This paper presents lab and field-validated methods for pipeline operators to accurately detect, size, and subsequently prioritize digs for Selective Seam Weld Corrosion (SSWC) defects with direct imaging ILI technology. Building on the complex crack and corrosion morphologies mapping capabilities of direct imaging ILI technology introduced by Simpson et al. at PPIM 2025 and 2026, the technology is further advanced and applied to SSWC features. The increased resolution and combined direct metal loss and crack inspection abilities are shown to be particularly advantageous in differentiating SSWC anomalies from generalized corrosion interacting with the long seam. The unified multimodal inspection capabilities of direct imaging ILI technology presented in this paper accurately measure both the general wall loss over long seam welds and the characteristic sharp, narrow grooving feature along the weld. This single-run method overcomes the limitations of inferred or amplitude-based methods and data registration challenges used in legacy ILI tools. Detailed in this paper is a comprehensive method to evaluate SSWC across its full range of morphological components, from general corrosion and preferential weld-seam grooving to coincident cracking. Lab validation and field in-ditch NDE dig results across a wide range of groove widths, depths, aspect ratios, and sharpness are presented. Direct imaging ILI is applied to:- Clearly differentiate general corrosion occurring on or near a long seam from true preferential corrosion along the weld bondline.- Accurately size grooving in the weld seam and simultaneously evaluate for crack-like features extending beneath it. - Identify locations with high potential for future SSWC growth by resolving shallow corrosion from coating failure and water ingress. A variety of field digs and NDE results are compared to direct imaging ILI findings and presented as case studies supporting the methodology derived in the lab validation phase. Recommendations are presented to further improve the evaluation and prioritization of SSWC features through ILI inspection methods. Keywords for subject area: ILI Application, Selective Seam Weld Corrosion, SSWC, Crack, Metal Loss, Direct Imaging
Available after the event